5. The moisture content of the pigment in the paint is too high or mixed with water during construction. Prevention: The moisture content of the pigment should be controlled and water should not be mixed during construction.
6. Excessive amount of diluent used in construction or high-boiling thinner such as kerosene. Prevention: The amount of diluent should not be too much, and the addition of high boiling point solvents such as kerosene should be avoided.
7. Rain or dew before the coating film is completely dry. Prevention: The film should be protected from rain or dew during the drying process.
According to the above analysis, it can be seen that the construction technology and habits of Zhejiang floor paint are one of the important reasons for the loss of light. The construction technology and construction environment requirements of the standard are established. The operation of the standard construction process can avoid the prevention and control of Zhejiang floor paint. There is a chance of losing light.
Please contact Home Decoration Spc Vinyl Flooring Supplier get more information with spcfloors@gmail.com.